EN8 Chemical Composition
| Element | Range (per standard) |
|---|---|
| Carbon (C) | 0.36 – 0.44 % |
| Manganese (Mn) | 0.60 – 1.00 % |
| Silicon (Si) | 0.10 – 0.40 % |
| Sulphur (S) | 0.050 % max |
| Phosphorus (P) | 0.050 % max |
Reference ranges vary by standard revision and exact designation. Confirm the purchase specification and use the Mill Test Certificate for the supplied heat.
EN8 Properties & Condition
| Property | Typical Value |
|---|---|
| Tensile Strength | 550 – 700 MPa |
| Typical Condition | Normalised |
| Machinability | Good in normalised condition |
| Weldability | Weldable with preheat |
Mechanical properties depend on heat-treatment condition and section size. Confirm the required values against the governing order specification before purchase.
Key Characteristics of EN8
- Higher tensile strength and wear resistance than IS 2062 mild steel
- Responds to flame and induction hardening on the surface
- Readily machined in the normalised condition
- Cost-effective where alloy content is not justified
EN8 Applications
- General machinery shafts and spindles
- Connecting rods and axle shafts
- Studs, bolts, keys and drive couplings
- Gear blanks for lightly loaded drives
How we supply EN8
Carbon Rods
High-tensile forged and peeled bars in EN8 and EN9 grades. Normalized for uniform machinability.
Carbon SteelMS Rounds
Bright and black finish steel rounds in standard lengths and custom cut pieces for general fabrication.
ProcessingHacksaw Cutting
High-precision cut-to-size material processing with ±1mm tolerance. Zero workshop wastage.
Buyers also compare
Calculate EN8 tonnage
Estimate theoretical bar weight before you raise the enquiry.
Open Steel Weight Calculator →Direct Yard Desk
Kalpesh & Ritesh Shah
Darukhana, Mazgaon, Mumbai
Mobile: +91 98200 23666
Hours: Monday to Saturday, 9:00 AM to 7:00 PM IST